Stress corrosion cracking in October 2018 led to pipeline rupture near Prince George

Updated story 11:22 AM

Stress corrosion cracking led to the 2018 Enbridge pipeline rupture 13 kilometres northeast of Prince George.

According to the Transportation Safety Board (TSB), deficiencies in predicting the extent of the cracking and a deferred inspection led to a hazard being undetected prior to the rupture.

The inspection was scheduled for 2017 but was deferred until the fall of 2018, meaning the existing cracks went undetected.

TSB Senior Investigator, Jennifer Philopoulos told MyPGNow.com this decision played a big role in the rupture.

“There is a likelihood that if the inspection had been done in 2017, and the inspection technology that would have been used would have captured the size of the crack, that would have been present at that time.”

Enbridge Senior Vice-President and Chief Operations Officer for the Gas and Midstream Business, Michele Harradence stated the company is doing all it can to regain the trust of the surrounding community and the Lheidli T’enneh.

“We want to work with the Chief-and-council to build a positive and mutually beneficial relationship and we want to see how we can build those shared priorities of safety, environmental protection, and economic development.”

Harradance adds Enbridge is chalking this up as a learning experience.

“We know this incident has caused concern and disrupted the lives of many people in the area and we absolutely apologize for that. We are very committed to have learned from this incident and we are taking steps to ensure the safety of our natural gas system.”

Since the explosion took place, Enbridge has completed a comprehensive pipeline integrity program on its natural gas pipeline system in BC to prevent similar incidents in the future.

“It’s actually the most aggressive program we have ever done on a system in BC and is aggressive as you’ll find in our industry. It’s really part of a new approach to pipelines and safety across all of our gas transmission assets,” added Harradence.

In February of 2019, the Lheidli T’enneh filed a lawsuit against Enbridge following the pipeline burst.

The host first nation claimed inadequate communication and the lack of emergency response from Enbridge was two of the main reasons behind the lawsuit.

====

Original Story 8:13 AM

The Transportation Safety Board has unveiled its report outlining the Enbridge Pipeline rupture and fire near Prince George in October in 2018.

The organization found that stress corrosion cracking led to the rupture resulting in the blaze.

Deficiencies in predicting the extent of the cracking and a deferred inspection led to a hazard being undetected prior to the rupture according to the TSB.

Following the rupture, the natural gas being transported was released and ignited.

No injuries were reported but 125 residents within a two-kilometre radius were evacuated.

In February of 2019, the Lheidli T’enneh filed a lawsuit against Enbridge following the pipeline burst.

The host first nation claims inadequate communication and the lack of emergency response from Enbridge were two of the main reasons behind the lawsuit.

In December, it was announced that the Enbridge West Coast Pipeline is operating at full capacity.

Something going on in the Prince George area you think people should know about?
Send us a news tip by emailing [email protected].

Brendan Pawliw
Brendan Pawliw
Since moving to Prince George in 2015, Brendan has covered local sports including the WHL’s Prince George Cougars, Prince George Spruce Kings, UNBC Timberwolves, Cariboo Cougars AAA, and Northern Capitals U18 female hockey teams. Career highlights include play-by-play during the Spruce Kings' BCHL championship runs in 2018 and 2019, including the Doyle Cup win. He also covered the 2019 National Junior A Championship, the 2017 Telus Cup, the 2022 World Women’s Curling Championship, and the 2022 BC Summer Games. Brendan is the news voice on 94.3 The Goat and Country 97 FM, reporting on crime, real estate, labour, and environmental issues. Outside of work, he officiates box lacrosse and fastball, sits on the Prince George Sports Hall of Fame board, and co-hosts the Hockey North podcast.

Continue Reading

cjci Now playing play

cirx Now playing play

- Advertisement -

Related Articles

- Advertisement -

Latest News

Hartley’s Sports Shorts; Monday, September 22nd

WHL:Prince George Cougars  7  Portland Winterhawks  2  (Saturday)The Cougars took control early for the second consecutive night by scoring three goals in each of the first two periods in front of 3,764 fans at CN Centre.

City Council waiting for more information before saying yes to World Cup watch parties

Prince George City Council has decided to wait for more information before making a decision on hosting watch parties for the 2026 FIFA World Cup.At Wednesday's meeting, City Council discussed a notice of motion put forward by Councillors Ron Polillo and Cori Ramsay, directing staff to work with a few local organizations to plan and execute outdoor watch parties to be held at Canada Games Plaza. 

Mounties host block parties to re-engage Block Watch programs

The Prince George RCMP hosted a Block Watch Part at Shas Ti Kelly Road yesterday (Saturday). This was one of four Block Watch Parties to be put on by the RCMP, each of them encompassed different parts of the city.

Darin’s Sports Shorts; Sunday, September 21st

Recap of local and national sports.

New-look Cougars sink their teeth into Portland

The Cougars find themselves off for the next 12 days before heading to Spokane for a two-game set against the Chiefs October 3rd and 4th.
- Advertisement -